1
Tensile strength
At a speed of 100mm/min, the tensile resistance F ≥ 22KN.
2
Fatigue test
Tests are conducted in a neutral environment in accordance with GB/T 10125 standards, requiring no white rust after 72 hours and no red rust after 96 hours.
3
High and low temperature test
After the part is placed at 100℃±3℃ for 24 hours and at -40℃±3℃ for 24 hours, it shall not deform, crack, or show obvious changes on the surface.
4
Dynamic test
Dynamic tests are conducted in accordance with GB 14166, requiring that the latch tongue must not have problems such as breaking or peeling.